Precise analysis for duplex steel

The development of duplex steels began in the 1970s and their use has steadily increased. Especially in the oil and gas industry, for chemical tankers, in the paper industry and for water systems, where the content of much more expensive nickel can be reduced through addition of nitrogen and as a result, production costs can be lowered. This has meant that the production of duplex steels has more than doubled in the last decade. However, due to the use of duplex steels in applications that are critical for safety, their quality must be strictly controlled. Optical emission spectrometry (OES) technology provides precise material verification and positive material identification (PMI) in order to prevent fatal consequences of material mix-ups. 

Duplex, super-duplex and hyper-duplex steels consist of an austenitic and ferritic structure, hence the designation “duplex”, and are classified as stainless steels. They set themselves apart with high structural stability, outstanding weldability characteristics and excellent corrosion resistance.

Elements

C %

Cr %

Ni %

Mo %

N %

Duplex

<0.03

~20

~5

~3

0.08 – 0.22

Super-duplex

<0.03 

~25

~7

 ~4

0.15 – 0.4

Hyper-duplex

<0.03 

~30

~7,5

 ~4

0.3 – 0.6

Average composition of typical duplex, super-duplex and hyper-duplex steels.

The important role of OES

A characteristic of duplex steels is the elevated nitrogen content, which considerably increases their corrosion resistance and solid solution strengthening due to pronounced austenite formation. Duplex steels are therefore easy to identify by means of the nitrogen content. On site, this is only possible with OES technology. Whilst in the laboratory, the advantages of OES compared to the combustion method include considerably easier specimen preparation, full analysis and much lower operating costs.

In cases where analysis in the laboratory is not possible (e.g. unwieldy items, petrochemical plants), the PMI-MASTER Smart portable spark spectrometer in combination with a UVTouch smart probe from Hitachi High-Tech Analytical Science for example can be used to conduct a high-performance analysis on site, including measuring nitrogen. Analysis at close to laboratory level is possible thanks to the patented optics in lightweight construction, dynamic spectrum evaluation and optimised excitation.

In a laboratory, the smallest stationary OES analyzer, like the FOUNDRY-MASTER Smart, has a working range of 0.05 – 1.2% and a precision level otherwise seen only in far larger spark spectrometers.

The basics of duplex steel composition

Four alloying elements are responsible for the key properties: Chromium (Cr), Molybdenum (Mo),

Nitrogen (N) and nickel (Ni). Cr is a ferrite former and provides the necessary corrosion resistance even at elevated temperatures. Mo supports the Cr effects and increases drastically the resistance against pitting and crevice corrosion in chloride containing environment. Although it’s also a ferrite former, its concentration is usually limited at 7.5% max.

Although nitrogen is a cheap alloying element, it has a major influence on the properties. N supports the corrosion resistance and increases substantially strength and toughness of the duplex steel. It has another important role during fabrication by delaying intermetallic phase forming and therefore conserving the dual microstructure during the production steps. As a strong austenitic former it could replace some expensive nickel in the alloy.

Lastly, Ni is the austenitic stabilizer which promotes the change of the crystal structure from body centred cubic (ferritic) to face-centred cubic (austenitic). A typical chemical composition of duplex steel (1.4462, S32205): C 0.03% Cr 22.5% Ni 5.0% Mo 3.25% N 0.18%.

Guido Odenthal, from Odenthal’s Engineering Office, which is an accredited test laboratory, commented: “Due to their better corrosion resistance and higher strength, duplex and super-duplex steels are being used more and more often in apparatus and pipeline construction over the last few years, either as base materials or also for the entire welded structures. Since duplex steel is easy to distinguish based on the nitrogen content, we use a spark spectrometer from Hitachi High-Tech for testing.”

Find out more about our spark spectrometer range or contact us to arrange your expert demo. One of our experts with assesses your specific requirements and recommend the right products for your business.

Find out more Get in touch


You might also be interested in:

Our full range of spark OES instruments
View an on-demand spark OES demo
Book a 1:1 live demo




Share this blog

Date: 26 February 2018

Author: Michael Molderings, OES Product Manager

Share this blog

Blogs


How to comply with sulfur cap 2020

Read More
Bunting-Redditch chooses Hitachi’s X-MET8000 for laboratory testing

Bunting-Redditch chooses Hitachi’s X-MET8000 for laboratory testing

Read More
Quality assurance at Kugellagar-Express

Bearing excellence: quality assurance at Kugellagar-Express

Read More