Oxford, UK, 22 May 2018: Hitachi High-Tech Analytical Science Corporation (Hitachi High-Tech Analytical Science), a Hitachi High-Technologies Corporation (TSE: 8036) wholly owned subsidiary engaged in the manufacture and sales of analysis and measuring instruments, has launched a new solution dedicated to the field-portable analysis of bunker fuel. The new X-MET8000 Optimum solution provides ship owners and port state control an alternative, portable option to benchtop XRF (X-ray Fluorescence) analysers to measure and monitor sulfur content in bunker fuel to meet the legislative requirements of the International Maritime Organisation’s global 2020 sulfur cap.

The X-MET8000 Optimum handheld XRF analyser can be easily taken from site to site and ship to ship. The instrument is factory-calibrated with a sulfur range of 0% to 5%, and calibrated to ASTM , D4294, IP336 and ISO8754. The solution also provides the end-user everything they need to carry out the analysis easily: sample cups, safety window and film, light stand and safety shield, and a brand new sample tray to keep the cup and safety window stable during the analysis. With the X-MET, you can achieve real-time data transfer with our IOS and Android apps, and cloud service. It also has an embedded GPS to pinpoint where the analysis was performed to provide compliance reporting.

The new X-MET8000 handheld XRF solution complements Hitachi High-Tech’s existing laboratory-based sulfur analysers, LAB-X and X-Supreme, to provide ship owners and port state control flexibility. Analysis can be carried out on-board a vessel by ship owners either using a benchtop or handheld XRF analyser, whilst port state control has the option of using benchtop analysers in laboratories and handheld analysers to perform spot-checks onboard vessels to ensure compliance.

Christelle Petiot, Hitachi Product Business Development Manager, said: “Ensuring compliance with the 2020 global sulfur cap regulation is a challenge for many organisations and for the industry. On-board testing is the most effective method to establish compliance. We’ve got a long history working with testing houses in ports and laboratories. The launch of our X-MET8000 Optimum solution compliments our LAB-X benchtop analyser, which has been used over the last 20 years to test sulfur in fuel. We’ve recently launched a new model, the LAB-X5000. It’s the fastest, easiest to use and most versatile model in the range’s 45 year history.

“Our launch of the LAB-X5000 and X-MET8000 Optimum solution demonstrate how we are constantly evolving our product ranges to ensure ship owners and port authorities are able prove their compliance now and in the future.”


In 2020, the IMO will enforce a new global sulfur limit of 0.5% for bunker fuel oil. You can make sure you meet the current and new global sulphur limits with our analysers. Download our whitepaper today to find out more...

 

Find out more

Date: 22 May 2018

Author: Hitachi High-Tech Analytical Science

News


Hitachi High-Tech sets a new pace for plating and coatings analysis with the new FT230

Read More

Hitachi High-Tech Analytical Science Growing Its Product Line with Thermal Analysis in the Americas Region

Read More

Hitachi High-Tech opens new state-of-the-art production facility in Shanghai, China

Read More

Global

Laura Phimister

Global Marketing Communications Manager, Global

EMEA

Jin-Joo Kim

Marketing Communications Manager, EMEA

Americas

Abigail Sheckler

Marketing Communication Specialist, Americas

Asia

Neha Karnik

Marketing Communications Manager, Asia

China

Jinnee Ni

Marketing Communications Manager, China