Fast, accurate, lab quality analysis in the palm of your hand.

See More

X-MET8000 Handheld Analyzer


Versatile materials analyzer

Testing a vast range of materials – solids, powders or liquids – the X-MET8000 is ideal for analysing metals, soils, wood, plastics, glass, oils and more. The analysis is non-destructive and leaves no test mark.

Anyone can work it anywhere

Lightweight, compact and portable, the X-MET8000 is operated by an icon-based touch-screen and comes pre-calibrated for many applications. Easy to use and its military-grade durability is more than a match for the dirtiest, hottest and most hostile environments. In addition, an optional window shield can protect the detector from sharp and rough materials.

Precision in an instant

X-MET8000 can provide results on site in seconds, depending on the application. Phenomenal reliability and speed, with no requirement to return for lab assessment, mean optimum productivity, lower costs and an all-important edge over your competitors.  Data can be stored on the analyser, on a USB flash drive, or through our app and cloud service for immediate sharing.

Contact us to find out more about X-MET8000

We send out regular marketing news, updates, promotions and offers by email. Please let us know if you would like us to contact you by email or not, by selecting one of the options below. *

The X-MET8000 Handheld XRF Analyser Won't Let You Down

Compare X-MET8000 Models

X-MET8000 Smart
  • X-ray tube : 40kV
  • X-ray tube filters: Single
  • Detector: Large area SDD
  • Max. sample temperature : 100ºC
  • IP54 rating
  • Protection against detector window damage : Window shield
  • Calibrations : Standardless (FP)
  • Integrated camera (Optional)
Get a quote
X-MET8000 Optimum
  • X-ray tube : 40kV or 50kV
  • X-ray tube filters: 6 position filter changer
  • Detector: Large area SDD
  • Max. sample temperature : 100ºC or 400ºC with HERO™ heat resistant window (optional)
  • IP54 rating
  • Protection against detector window damage : Optional window shield
  • Calibrations : Standardless (includes light elements analysis)
  • Integrated camera (Optional)
  • Small-spot collimator (Optional)
  • 6-position filter wheel for the optimised analysis of all elements from Mg to U
Get a quote
X-MET8000 Expert
  • X-ray tube : 50kV
  • X-ray tube filters: 6 position filter changer
  • Detector: Large area SDD
  • Max. sample temperature : 100ºC or 400ºC with HERO™ heat resistant window (optional)
  • IP54 rating
  • Protection against detector window damage : Optional window shield
  • Calibrations : Standard + automatic selection of empirical calibrations (traceable to certified reference materials)
  • Integrated camera
  • Small-spot collimator (Optional)
  • 6-position filter wheel for the optimised analysis of all elements from Mg to U
Get a quote

Contact Us

Complete your details, to find out more, request a demo, or get a quote.

We send out regular marketing news, updates, promotions and offers by email. Please let us know if you would like us to contact you by email or not, by selecting one of the options below. *